WF6 refers to tungsten hexafluoride, a chemical compound composed of one tungsten atom bonded to six fluorine atoms. Here are some key points about WF6:
| Test items | Units | Quality requirements | Test results |
| CF4 | ppm | <0.5 | <0.01 |
| O2 | ppm | <0.5 | <0.01 |
| N2 | ppm | <1 | 0.03 |
| CO | ppm | <0.5 | <0.02 |
| CO2 | ppm | <0.5 | <0.01 |
| SiF4 | ppm | <0.5 | <0.1 |
| SF6 | ppm | <0.5 | <0.1 |
| HF | ppm | <5 | 0.19 |
| Al | ppb | ≤10 | <0.020 |
| As | ppb | ≤10 | <0.001 |
| B | ppb | ≤10 | <0.005 |
| Ca | ppb | ≤5 | <0.200 |
| Cd | ppb | ≤2 | <0.001 |
| Cr | ppb | ≤10 | <0.020 |
| Fe | ppb | ≤10 | <0.007 |
| K | ppb | ≤5 | <0.100 |
| Mn | ppb | ≤10 | <0.001 |
| Na | ppb | ≤5 | <0.040 |
| Th | ppb | ≤0.1 | <0.001 |
| Ti | ppb | ≤10 | <0.002 |
| Li | ppb | ≤10 | <0.002 |
| U | ppb | ≤0.05 | <0.001 |
| Zn | ppb | ≤10 | <0.005 |
| Si | ppb | ≤10 | <0.100 |
| Pb | ppb | ≤10 | <0.001 |
| P | ppb | ≤2 | <0.300 |
| Mg | ppb | ≤10 | <0.020 |
| Ni | ppb | ≤20 | <0.030 |
| Cu | ppb | ≤5 | <0.005 |
| Mo | ppb | ≤10 | <0.001 |
| Total impurities of other metal | ppb | ≤500 | <0.0010 |
Detailed Photos
![]()



| MOQ: | 1 Piece |
| Price: | US $ 15/PC |
| Standard Packaging: | Cylinder/Tank |
| Delivery Period: | 15 days |
| Payment Method: | L/C, T/T |
| Supply Capacity: | 200 Tons/Year |
WF6 refers to tungsten hexafluoride, a chemical compound composed of one tungsten atom bonded to six fluorine atoms. Here are some key points about WF6:
| Test items | Units | Quality requirements | Test results |
| CF4 | ppm | <0.5 | <0.01 |
| O2 | ppm | <0.5 | <0.01 |
| N2 | ppm | <1 | 0.03 |
| CO | ppm | <0.5 | <0.02 |
| CO2 | ppm | <0.5 | <0.01 |
| SiF4 | ppm | <0.5 | <0.1 |
| SF6 | ppm | <0.5 | <0.1 |
| HF | ppm | <5 | 0.19 |
| Al | ppb | ≤10 | <0.020 |
| As | ppb | ≤10 | <0.001 |
| B | ppb | ≤10 | <0.005 |
| Ca | ppb | ≤5 | <0.200 |
| Cd | ppb | ≤2 | <0.001 |
| Cr | ppb | ≤10 | <0.020 |
| Fe | ppb | ≤10 | <0.007 |
| K | ppb | ≤5 | <0.100 |
| Mn | ppb | ≤10 | <0.001 |
| Na | ppb | ≤5 | <0.040 |
| Th | ppb | ≤0.1 | <0.001 |
| Ti | ppb | ≤10 | <0.002 |
| Li | ppb | ≤10 | <0.002 |
| U | ppb | ≤0.05 | <0.001 |
| Zn | ppb | ≤10 | <0.005 |
| Si | ppb | ≤10 | <0.100 |
| Pb | ppb | ≤10 | <0.001 |
| P | ppb | ≤2 | <0.300 |
| Mg | ppb | ≤10 | <0.020 |
| Ni | ppb | ≤20 | <0.030 |
| Cu | ppb | ≤5 | <0.005 |
| Mo | ppb | ≤10 | <0.001 |
| Total impurities of other metal | ppb | ≤500 | <0.0010 |